Raw Material
We support our customers in the development of their projects with the commitment to optimise the efficiency of their production through process improvement.
Home / Raw Material
The manufacturing process uses pure zinc, with at least 99.995% in accordance with the standard
UNE EN 10204:2006 and EN 1179: 2003 Z1
Such prerogative guarantees the maximum quality in the production of the zinc wire.
Technical specifications:
Chemical Analysis EN 1179: 2003 Z1
Chemical Analysis EN 1179: 2003 Z1
- Minimum of Zinc 100,00%.
Impurities
- Lead ppm 30
- Cadmium ppm 30
- Tin ppm 10
- Iron ppm 20
- Copper ppm 10
- Aluminium ppm 10
- Total Impurities ppm 50
We export to all countries.
Physico-Mechanical Analysis
- Mass / Volume Klg/dm3 7,14
- Melting Point (Liquid) ° C 419
- Boiling temperature ° C 907
- Elongation % 50-95
- Tensile strength mpa 95-130 (according to customer's requirements)
Diameters from 1.60 to 6.00 mm
Packing on pallets 560 x 1100 mm with two barrels (cardboard or metal)
with 250 Klg / 300 Klg / 500 Klg each
We export to all countries.